Views: 0 Author: hbkaishi Publish Time: 2023-12-20 Origin: hbkaishi
Wrinkling treatment method for stainless steel tensile parts
一. Analysis of causes of wrinkles
1. Uneven pressure
In drawing processing, if the cutting speed is too fast or the machine tool processing is uneven, a slight extrusion force may be formed on the surface of the material, causing wrinkles.
2. Insufficient material strength
Wrinkling can also occur if the strength of the material is lower than required for stretching.
3. Mold design defects
Insufficient considerations in mold design or imperfect mold manufacturing processes may result in ripples and wrinkles.
二. How to deal with wrinkles of stainless steel tensile parts
1.Material selection
Choose better quality stainless steel flanges or steel pipes to ensure that the strength meets the requirements.
2. Optimize process parameters
Reasonably adjust the stretching processing parameters to reduce wrinkles caused by uneven pressure. For example, you can reduce the cutting speed, increase the processing intensity, and correctly control the processing gap.
3.Mold improvement
Sometimes it is necessary to improve the mold design or replace the mold with a better quality one to reduce the possibility of wrinkling. You can consider changing the angle and arc radius to optimize the process to avoid wrinkles.
4. Follow-up processing
If wrinkles still occur, subsequent treatments such as sanding or polishing can be used to remove the wrinkles and make the product surface smoother and more uniform.