Common Defects of Stamping Parts Flanging

Views: 0     Author: KAISHI     Publish Time: 2025-01-24      Origin: Kaishi

Common Defects of Stamping Parts Flanging

Common defects of stamping parts flanging

Defects: flanging is not vertical, flanging height is inconsistent, flanging burrs, flanging cracks, etc.

1. Flanging is not vertical → the gap between the male and female dies is too large.

2. Flanging height is inconsistent → the gap between the male and female dies is uneven; positioning is inaccurate; the size of the blanking parts is inaccurate.

3. Flanging burrs → there are scars on the cutting edge; there are impurities on the surface of the parts; the hardness of the cutting edge is too low.

4. Flanging cracks → large burrs during trimming; the gap between the male and female dies is too small; there is a sudden change in the shape of the flanging.


About Our Company

Our experienced engineering team will provide you technical assistance to optimize your design and support your application to work out the best solution and control your purchasing cost.

QUICK LINKS

PRODUCTS

CONTACT US

:+86-137-2273-0310
:West Village, Xisanli Village, Nanpi Town, Cangzhou, Hebei, China
Copyright © 2023  Kaishi Hardware Manufacturing. All Rights Reserved.Privacy Policy